TPV Injection Moulding


Dryflex XL Injection Moulding Guidelines



Gates and Runners: Fully round allowing easy flow
Venting: 0.02 - 0.05mm deep at final fill point
Injection Speed: Medium - Fast
Injection Pressure: Medium
Back Pressure: Low - Medium
Holding Pressure: Sufficient to pack the mould
Cooling: Parts can be demoulded once temperature drops to approx. 100°C

 